ASTM D6099-97
Historical Standard: ASTM D6099-97 Standard Test Method for Polyurethane Raw Materials: Determination of Acidity in Moderate to High Acidity Aromatic Isocyanates
SUPERSEDED (see Active link, below)
ASTM D6099
1. Scope
1.1 this test method determines the acidity, expressed as parts per million (ppm) of HCI, in aromatic isocyanate samples of greater than 100-ppm acidity. The test method is applicable to products derived from toluene diisocyanate and methylene-bis(4-phenylisocyanate) (see Note 1).
Note 1- There is no similar or equivalent ISO standard.
2. Referenced Documents (purchase separately) The documents listed below are referenced within the subject standard but are not provided as part of the standard.
ASTM Standards
D883 Terminology Relating to Plastics
E180 Practice for Determining the Precision of ASTM Methods for Analysis and Testing of Industrial and Specialty Chemicals
E691 Practice for Conducting an Interlaboratory Study to Determine the Precision of a Test Method
ISO Standards
ISO14898 Plastics--Aromatic isocyanates for use in the production of polyurethane--Determination of acidity Available from American National Standards Institute (ANSI), 25 W. 43rd St., 4th Floor, New York, NY 10036, http://www.ansi.org.Keywords
acidity; aromatic isocyanates; isocyanates; MDI; methylene diphenyldiisocyanate; polyurethane; raw materials; TDI; titration; toluene diisocyanate;
ICS Code
ICS Number Code 83.040.01 (Raw materials for rubber and plastics in general)
DOI: 10.1520/D6099-97